Deck: Blocking for the pop-up deck cleats was made from 3/4" marine grade plywood
Fits like a glove !
1. Blocking for the pop-up deck cleats was made from 3/4" marine grade plywood.
2. The cleat pops up when you hit the release button.
3. To restore some of the deck batten thickness we removed while fairing, we laminated a strip of 1/4" marine grade plywood to the underside of several battens.
4. The battens will be encapsulated before applying the plywood deck.
Deck: Fill coat # 1 : We blocked out the seams with coarse sandpaper and airfiled the surface wi
Fill coat # 2 : The second fill coat was applied at 1 AM. Another late night !
1. Fill coat # 1: We blocked out the seams with coarse sandpaper and airfiled the surface with 80 grit sandpaper. The first round of West System 105 Resin catalyzed with 206 Medium Hardener was applied at 7 PM.
2. We'll let it cure for a day or two before doing some fairing.
12